Gold - dry nanopowder, hydrophobic, 2 nm
Forms colloidal solutions in non-polar solvents. Monodisperse nanoparticles, can be used for 2-D and 3-D structures build-up.
Compare products with technical highlights, document cues, and product details.

Forms colloidal solutions in non-polar solvents. Monodisperse nanoparticles, can be used for 2-D and 3-D structures build-up.

Forms colloidal solutions in non-polar solvents. Monodisperse nanoparticles, can be used for 2-D and 3-D structures build-up.

Colloidal solution in water, 0,05 mg/mL Average particle size: 20±3 nm (other sizes available upon request) pH ca. 8,0.

can be supplied at higher Au-concentrations too (*Au concentration in colloid according to extractive photometric determination with 1-(2,4,6-trichlorophenyl)-4,4,6-trimethyl- (1H,4H)-2-Pyrimidinethiol, see M. A. ANUSE et al., Talanta. Vol. 32, No. 10, pp. 1008-1010, 1985) Optical density at maximum after dilution x 30 times: 0.5± 0.01 Particle size, average (TEM): 14±3 nm Adsorption maximum position: 524 nm ± 2 nm.

Au concentration: 0,05 mg/mL (corresponds to 0,01% HAuCl4), aq. solution Admixtures, %: tannic acid < 0,01; sodium citrate < 0,04.

Au concentration: 0,05 mg/mL (corresponds to 0,01% HAuCl4), aq. solution Admixtures, %: tannic acid < 0,01; sodium citrate < 0,04.

Au concentration: 5 mg/mL, aq. solution Admixtures: citrate, cell-culture bovine gelatine.